MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) Kalix® 2940 High Performance (HPPA)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: Kalix® 2940 is a bio-sourced, polyamide-based compound with 40% by weight glass fiber reinforcement. This material is specifically formulated for high strength and stiffness applications where good impact resistance and excellent dimensional stability after molding are required. The formulation also addresses warpage issues associated with the anisotropic shrinkage of glass fiber reinforced materials so that close tolerance molding is more easily achieved. Its low viscosity and excellent flow properties make the material ideal for filling parts with thin-walled sections such as those encountered in the mobile electronics industry.

Applications: Cell Phones; Electrical Parts; Electrical/Electronic Applications; Thin-walled Parts

Features: Fast Molding Cycle; Good Dimensional Stability; Good Impact Resistance; Good Surface Finish; High Flow; High Stiffness; High Strength; Hot Water Moldability; Low Warpage; Paintable; Platable

Typical values shown tested on Dry as Molded samples.

Standard Packaging and Labeling:
- Kalix® resin is packaged in foil lined, multiwall paper bags containing 25 kg (55 pounds) of material. Individual packages will be plainly marked with the product number, the color, the lot number, and the net weight.

Injection notes: Storage:
- Kalix® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Kalix® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Kalix® processing guide.
Drying:
- Kalix® is supplied in sealed bags. It should be dried before molding because excessive moisture content will result in reduced mechanical properties and processing issues, such as excessive nozzle drooling, foaming and splay visible on the molded parts.
- Use of a desiccant dryer with -40°C dewpoint is strongly suggested to ensure Kalix® material has reached optimum moisture content before processing.
Injection Molding:
- Set injection pressure to give rapid injection. Adjust holding pressure to one-half injection pressure. Set hold time to maximize part weight. Transfer from injection to hold pressure at the screw position just before the part is completely filled.
- For light colors use lower melt temperature if possible. If operating in the 330°C melt temperature range, keep residence times below 5 minutes.
- Actual mold temperatures of 80°C or above are recommended to improve flow and part surface finish. The use of mold temperatures below 80°C is safe for mechanical properties but may result in higher necessary injection pressure and inferior surface finish.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/cc
Water Absorption 0.13 %
@Time 86400 sec
0.13 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0015 cm/cm0.0015 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0055 cm/cm0.0055 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress 175 MPa25400 psiISO 527-2
Elongation at Break 3.0 %3.0 %ISO 527-2
Tensile Modulus 13.0 GPa1890 ksiISO 527-2
Flexural Strength 290 MPa42100 psiISO 178
Flexural Modulus 11.0 GPa1600 ksiISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²Type 1, Notch A; ISO 180
Izod Impact, Unnotched (ISO) 80.0 kJ/m²38.1 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.62
@Frequency 1e+6 Hz
3.62
@Frequency 1e+6 Hz
ASTM D150
 3.83
@Frequency 1000 Hz
3.83
@Frequency 1000 Hz
ASTM D150
Dissipation Factor  0.012
@Frequency 1000 Hz
0.012
@Frequency 1000 Hz
ASTM D150
 0.012
@Frequency 1e+6 Hz
0.012
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 223 °C433 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 218 °C424 °FUnannealed; ISO 75-2/A
Glass Transition Temp, Tg 55.0 °C131 °FASTM E1356
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 265 - 300 °C509 - 572 °F
Middle Barrel Temperature 280 - 330 °C536 - 626 °F
Front Barrel Temperature 280 - 330 °C536 - 626 °F
Melt Temperature 280 - 330 °C536 - 626 °FInjection
Mold Temperature 50.0 - 130 °C122 - 266 °F
Drying Temperature 80.0 °C
@Time 14400 - 43200 sec
176 °F
@Time 4.00 - 12.0 hour
Moisture Content <= 0.090 %<= 0.090 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
ColorWhite
FormsPellets
ProcessingInjection Molding; Water-Heated Mold Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4303 / 280103

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.