MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ChevronTexaco Block Grease
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Chevron Block Grease is a high melting point block grease.

It is manufactured using highly refined base oils, a lithium thickener, and a special oxidation inhibitor which eliminates glazing and charring. It is fibrous-textured and dark brown in color

Chevron Block Grease has good lubricant film retention and, thus, assures low starting torque and reduced friction during operation. Its uniform consistency and hardness throughout each block assures that the lubricant is fed evenly at a constant rate.

Chevron Block Grease lubricates well in applications where operating temperatures up to 149°C are encountered. It is non corrosive to bronze bearings.

Applications

Chevron Block Grease is recommended for all bearings with open grease cellars, such as those on older kilns, rod and ball mills, laundry equipment, kiln cars, dehydrators, etc

Key Words: CPS Number: 253500; MSDS Number: 1184
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 6262Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 1427 SUS1427 SUS
Saybolt Viscosity at 210°F 91 SUS91 SUS
Kinematic Viscosity at 40°C (104°F) 265 cSt265 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 17.5 cSt17.5 cStASTM D445
 
Mechanical PropertiesMetricEnglishComments
Penetration P(0), 1/10 mm 4040
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air 21.0 °C69.8 °F
Flash Point 230 °C446 °FASTM D92
Dropping Point 190 °C374 °F
 
Descriptive Properties
ColorDark Brown
TextureFibrous
ThickenerLithium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco RPM® SAE 85W-140 Universal Gear Lubricant
ChevronTexaco RPM® SAE 75W-90 Synthetic Gear Lubricant
ChevronTexaco RPM® SAE 140 Gear Oil
ChevronTexaco Black Pearl® NLGI 1 Grease EP
Chesterton 629 High Temperature White Grease

WCHEV240 / 74855

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.