MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay SUPER CEROX™ 1663 Surfactant
Categories: Fluid

Material Notes: Description: Super Cerox™1663 is particularly suited for the polishing of ophthalmic lenses (mass production and prescription) and optical lenses.

Benefits: High polishing efficiency, Very high surface quality and Improved suspension properties

Features: Super Cerox™ 1663 is recognized in the ophthalmic market as a versatile product offering outstanding performance on various polishing equipments and conditions.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Loss On Ignition <= 1.0 %<= 1.0 %
Particle Size 1.0 - 2.0 µm1.0 - 2.0 µmD50 Sedigraph
 1.5 - 3.0 µm1.5 - 3.0 µmD50 Laser
 
Component Elements PropertiesMetricEnglishComments
CeO2 60 - 70 %60 - 70 %
 
Descriptive Properties
Content>90%TREO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay SUPRAGIL® GN 4-4’ Dihydroxydiphenyl Sulphonate Condensate Sodium Salt
Verdant Specialty Solutions ALKAMULS® 504/V Surfactant
Syensqo (Solvay Specialty Polymers) Clearbreak 343 Demulsifier
Syensqo (Solvay Specialty Polymers) Cerox™ 2822 Surfactant
Syensqo (Solvay Specialty Polymers) Cerox™ 2610 Surfactant

WRHOD106 / 137337

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.