Varcum 29709 is a two-step pulverized phenolic resin. APPLICATION: Varcum 29709 is recommended for use in the manufacture of bonded abrasives. FEATURES: - Excellent performance in grinding wheels which are to be used for both wet and dry grinding.
- Excellent resistance to the deteriorating effects of water based coolants.
Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |