MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Palm Labs Adhesives TURBO FUSE METHYL FOR METALS (75-95 Viscosity) Rapid Bonding Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Palm Lab's Methyl Cyanoacrylate is a one component rapid bonding adhesive ideal for metal surfaces. TURBO FUSE METHYL’s advanced formula is designed to polymerize instantly by absorbing surface moisture and is specifically formulated to bond various metals including aluminum, stainless steel, and copper, to itself and to a variety of materials including wood, balsa wood, rubber, plastics and leather. Applications include wiper blades, nameplates, gearshift indicators, aerospace parts, automotive and machinery parts, electronic components, transportation equipment, etc. Meets MLLA 46050 Type I Class II specification requirements.

Part Numbers for this data: 15-080Methyl, 30-080Methyl

Soluble in Acetone, MEK, Amide, Methylene Chloride

Information provided by Palm Laboratories Adhesives

Key Words: CAS No: 123-31-9
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccLiquid State
Viscosity 75 - 95 cPLiquid State
 
Mechanical PropertiesOriginal ValueComments
Shear Strength >= 725 psiABS; ASTM D1002/DIN 53283
 >= 1450 psiPolycarbonate; ASTM D1002/DIN 53283
 >= 1890 psiCopper; ASTM D1002/DIN 53283
 1890 - 2900 psiTensile, (Cured State)
 >= 2900 psiGrit Blasted Steel; ASTM D1002/DIN 53283
 >= 2900 psiEtched Aluminum; ASTM D1002/DIN 53283
 >= 2900 psiStainless Steel; ASTM D1002/DIN 53283
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.3Cured State; ASTM D150
Dielectric Strength 634.5 V/milCured; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°CASTM D696
Melting Point 160 - 170 °CCured State
Maximum Service Temperature, Air 180 °FCured State
Minimum Service Temperature, Air -60.0 °FCured State
Glass Transition Temp, Tg 120 °CASTM E228
Flash Point 176 - 200 °FLiquid State
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourCured State
Shelf Life 12.0 MonthLiquid State
 
Descriptive Properties
AppearanceClear liquidLiquid State
 Clear-HardCured State
Base compound (Resin)Methyl CyanoacrylateLiquid State
Chemical Resistance75% Initial Strength RetainedGasoline at 22°C, at 1000hrs
 80% Initial Strength RetainedGasoline at 22°C, at 500hrs
 85% Initial Strength RetainedIsopropanol at 22°C, at 500hrs
 85% Initial Strength RetainedIsopropanol at 22°C, at 1000hrs
 90% Initial Strength RetainedMotor Oil at 40°C, at 500hrs
 90% Initial Strength RetainedMineral Spirit at 22°C, at 500hrs
 90% Initial Strength RetainedMotor Oil at 40°C, at 1000hrs
 90% Initial Strength RetainedMineral Spirit at 22°C, at 1000hrs
Gap Fill0.20 mmCured State
Material Set Up Time10-15 secSBR to SBR
 10-20 secCopper to Copper
 10-30 secSteel to Steel
 15-20 secSteel to PVC
 30-60 secStainless Steel to Stainless Steel
 3-10 secPVC to PVC
 40-60 secAluminum to Aluminum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPALML021 / 135175

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.