MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Cabot CAB-O-SIL® ULTRABOND™ 5780 Fumed Silica
Categories: Other Engineering Material

Material Notes: Product highlights: CAB-O-SIL ULTRABOND 5780 fumed silica is a high-performing surface treated fumed silica. Compared to existing polydimethylsiloxane (PDMS) treated silicas, CAB-O-SIL ULTRABOND 5780 fumed silica imparts advantages in rheology control, adhesion, as well as aging properties to epoxy-based adhesives. CAB-O-SIL ULTRABOND 5780 fumed silica is especially suited for epoxy formulations that require excellent rheology control and storage stability. This product particularly allows stronger bonding of epoxy structural adhesives, such as Crash-Durable-Adhesives (CDA), to lubricated or oily metal substrates (steel, aluminum and other materials) used in Original Equipment Manufacturers’ (OEM) automotive production lines. These structural adhesives can address light-weighting, safety, durability, NVH (Noise, Vibration, and Harshness), manufacturing efficiency and sustainability requirements of the OEM.

Key applications: CAB-O-SIL ULTRABOND 5780 fumed silica is best suited for use in epoxy structural adhesives in a wide range of industries:

  • Automotive
  • Aerospace
  • Construction
  • Wind turbine blades

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Product FormPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT103 / 315838

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.