MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
NOVA Chemicals Sclair® 19K Resin Homopolymer HDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Features: high stiffness, excellent barrier properties, low gel. Additives: processing antioxidant.

Applications: barrier films, co-extrusion, dry food packaging, blending.

Film properties reported are typical of blown film extruded on a 2.5" extruder with 4" die and 35-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.958 g/ccASTM D 792
Moisture Vapor Transmission 2.64 cc-mm/m²-24hr-atm
@Temperature 38.0 °C
100% RH, atmospheric pressure; ASTM F1249
Oxygen Transmission Rate 1488 cc/m²/day
@Temperature 23.0 °C
ASTM D3985
Thickness 38.0 micronsAs tested
Melt Index of Compound 0.95 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 68ASTM D2240
Film Tensile Strength at Yield, MD 25.0 MPaASTM D882
Film Tensile Strength at Yield, TD 27.0 MPaASTM D882
Film Elongation at Break, MD 560 %ASTM D882
Film Elongation at Break, TD 890 %ASTM D882
Elmendorf Tear Strength MD 26 g
@Thickness 0.0380 mm
ASTM D1922
Elmendorf Tear Strength TD 711 g
@Thickness 0.0380 mm
ASTM D1922
Dart Drop Test 44.0 g
@Thickness 0.0380 mm
F50; ASTM D1709/A
Film Tensile Strength at Break, MD 42.0 MPaASTM D882
Film Tensile Strength at Break, TD 40.0 MPaASTM D882
1% Secant Modulus, MD 840 MPaASTM D882
1% Secant Modulus, TD 1180 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 131 °CASTM D 1525
 
Descriptive Properties
Low Friction Puncture20 J/mmNOVA Chemicals test

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOV602 / 249049

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.