MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron AboWeld 8104-12 Polysulfide-Epoxy Sealant and Caulk
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Polysulfide Sealant/Adhesive

Material Notes: AboWeld 8104-12 is a 2-part, 100% solids, liquid or filled polysulfide-epoxy. It is available in many colors. It is often used with sand and gravel to mix grouts for filling and resurfacing. It is primarily for strong adhesion on floors with heavy traffic.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 57 - 60
Tensile Strength at Break 200 - 220 psi
Elongation at Break 150 - 200 %
 
Processing PropertiesOriginal ValueComments
Cure Time 1440 - 4320 min(1-3 Days)
Pot Life 60 min
 
Descriptive Properties
ColorMany Colors
Parts by Weight (pbw)1Part B
 2Part A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP21TP-2 Two Component Polysulfide Epoxy Adhesive and Sealant
Abatron AboCast/AboCure 8007-2 High-Grade Polysulfide-Epoxy Flexible Membrane Sealant and Joint-Filler
Abatron AboSeal 8104-10 Polysulfide, Thixotropic or Self-Leveling Sealant and Caulk
Abatron AboSeal 8104-11 Polysulfide, Thixotropic Sealant and Caulk
Abatron AboSeal 8104-8 Polysulfide, Thixotropic Sealant and Caulk

PABC920 / 107904

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.