MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zircar Ceramics MB Alumina Blanket
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with temperatures as high as 1600° C (2912° F).

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.100 g/cc0.00361 lb/in³
Filament Diameter 2.0 - 4.0 µm2.0 - 4.0 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 0.0196 MPa>= 2.84 psiPerpendicular to Thickness
Resilience >= 5.0>= 5.0
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0700 W/m-K
@Temperature 315 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 599 °F
parallel to thickness; ASTM C177-76
 0.0900 W/m-K
@Temperature 540 °C
0.625 BTU-in/hr-ft²-°F
@Temperature 1000 °F
Parallel to thickness; ASTM C177-76
 0.130 W/m-K
@Temperature 760 °C
0.902 BTU-in/hr-ft²-°F
@Temperature 1400 °F
Parallel to thickness; ASTM C177-76
 0.170 W/m-K
@Temperature 980 °C
1.18 BTU-in/hr-ft²-°F
@Temperature 1800 °F
parallel to thickness; ASTM C177-76
 0.230 W/m-K
@Temperature 1200 °C
1.60 BTU-in/hr-ft²-°F
@Temperature 2190 °F
Parallel to thickness; ASTM C177-76
 0.300 W/m-K
@Temperature 1425 °C
2.08 BTU-in/hr-ft²-°F
@Temperature 2597 °F
Parallel to Thickness; ASTM C177-76
Maximum Service Temperature, Air 1600 °C2910 °F
Shrinkage  <= 1.0 %
@Temperature 1500 °C,
Time 86400 sec
<= 1.0 %
@Temperature 2730 °F,
Time 24.0 hour
Width and Length
 <= 3.0 %
@Temperature 1500 °C,
Time 86400 sec
<= 3.0 %
@Temperature 2730 °F,
Time 24.0 hour
Perpendicular to Thickness
 
Component Elements PropertiesMetricEnglishComments
Al2O3 80 %80 %
Fe2O3 <= 0.20 %<= 0.20 %
Loss on Ignition(%) <= 0.30 %<= 0.30 %
SiO2 20 %20 %
 
Descriptive Properties
Al2O3 + SiO2> 99.7
Alpha Al2O3< 5%
ColorWhite
Compressibility< 5%
Mullite50 to 70%
Shot Content0.04 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Cerafelt Refractory Fiber Felt
Morgan Advanced Ceramics Cerachrome™ Blanket Thermal Ceramic
Morgan Advanced Ceramics Cerachem™ Blanket Thermal Ceramic
Morgan Advanced Ceramics Cerablanket™ Thermal Ceramic
Morgan Advanced Ceramics Alphawool® Unifelt Thermal Ceramic

CZIR018 / 2826

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.