MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Henkel Loctite® Stycast® A 316-48 One-Component Oxide Filled Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Loctite Stycast A 316-48 provides the following product characteristics:
  • One component
  • Fast heat cure
  • Heat resistant
  • Non-conductive
  • Exceptional thermal stability
  • Excellent chemical resistance

Cure: Heat cure

Filler Type: Oxide

Application: Heat resistant adhesive

Typical Package Application: Sensors and Control modules

Surfaces: Plastics, Phenolics, Metals and Ceramics

Loctite Stycast A 316-48 is an oxide filled, pourable epoxy adhesive designed for use in harsh automotive applications.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/cc
Brookfield Viscosity 50000 cP50000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  40
@Temperature 130 °C
40
@Temperature 266 °F
 86
@Temperature 25.0 °C
86
@Temperature 77.0 °F
Tensile Strength 17.3 MPa2510 psiAluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  3.00e+13 ohm-cm
@Temperature 130 °C
3.00e+13 ohm-cm
@Temperature 266 °F
 1.00e+15 ohm-cm
@Temperature 25.0 °C
1.00e+15 ohm-cm
@Temperature 77.0 °F
Dielectric Constant 3.75
@Frequency 1000 Hz
3.75
@Frequency 1000 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear  55.0 µm/m-°C
@Temperature <=145 °C
30.6 µin/in-°F
@Temperature <=293 °F
Below Tg; ISO 11359-2
 155 µm/m-°C
@Temperature >=145 °C
86.1 µin/in-°F
@Temperature >=293 °F
Above Tg; ISO 11359-2
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 180 °C356 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg 145 °C293 °FISO 11357-2
 
Processing PropertiesMetricEnglishComments
Cure Time  0.960 min
@Temperature 160 °C
0.0160 hour
@Temperature 320 °F
Option 4. Post Cure: 2 to 4 hours at the highest expected use temperature
 3.00 min
@Temperature 140 °C
0.0500 hour
@Temperature 284 °F
Option 3. Post Cure: 2 to 4 hours at the highest expected use temperature
 4.98 min
@Temperature 120 °C
0.0830 hour
@Temperature 248 °F
Option 2. Post Cure: 2 to 4 hours at the highest expected use temperature
 30.0 min
@Temperature 100 °C
0.500 hour
@Temperature 212 °F
Option 1, Post Cure: 2 to 4 hours at the highest expected use temperature
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHENK7941 / 255426

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.