MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem AKROFLON 5R PTFE
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Akroflon 5R is a white free-flowing PTFE micropowder. The powder is designed for use as an additive in elastomers or plastics where improved lubricity and/or wear resistance is required. PTFE powders can withstand temperatures as high as 260°C (500°F). Akroflon 5R meets FDA requirements of 21 CFR 175.105, 175.300, 176.170, and 176.180.

Applications: Akroflon 5R used in elastomeric parts provides slip (low CoF), non-stick, water repellency, release, rub and abrasion resistance to surfaces. Typically, 5 to 50% (by weight) can be added to elastomeric compounds to achieve the desired properties. Improvements in tear strength, abrasion resistance and flex life have been measured when 10 phr or more of Akroflon 5R are incorporated in fluoro-elastomers, fluoro-silicones, EPDM, neoprene and SBR elastomeric compounds. Akroflon 5R is also recommended for use in water-based, solvent-based, powder and UV coatings, and offset and liquid inks.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 5.0 µmAverage
 
Thermal PropertiesOriginal ValueComments
Melting Point 320 °C
 
Descriptive Properties
Appearancewhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH336 / 315254

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.