MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 275H Nylon 6, Copolymer, Impact Modified
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Notes: Very high impact and elongation, low flexural modulus material for tubing and wire jacketing applications requiring a soft, flexible product; FMVSS Flammability: Passes, FMVSS 302

Processing Method: Extrusion; Injection Molding

Forms: Pellets

Automotive Specifications: Chrysler MS-DB41 Type PA CPN2785 Color: BK001 Black; Ford ESB-M4D423-A2; Ford ESF-M4D423-A; Ford ESB-M4D426-A; GM GMP.PA6.003; GM GMP.PA6.004; Packard M-2170

Information Provided by Teknor Apex

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/ccASTM D792
Linear Mold Shrinkage 0.015 - 0.020 in/inASTM D955
Melt Flow 3.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 6500 psiASTM D638
Elongation at Break 250 %ASTM D638
Flexural Strength 4000 psiASTM D790
Flexural Modulus 10000 psiASTM D790
Izod Impact, Notched 19.0 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 417 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 290 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °FUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 420 - 455 °F
Middle Barrel Temperature 445 - 485 °F
Front Barrel Temperature 465 - 490 °F
Nozzle Temperature 465 - 490 °F
Melt Temperature 465 - 490 °FProcessing Temperature
Drying Temperature 175 °F
Moisture Content 0.15 %
 
Descriptive Properties
Suggested Regrind, max25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Selar® PA 3426 Nylon Barrier Resin
Teknor Apex Chemlon 275 Nylon 6, Copolymer Impact Modified
LNP Konduit® ITF-212-11 Polyamide 6/12 Copolymer
Celanese Zytel® ST801 NC010A PA66-HI
Teknor Apex Chemlon® 104 Nylon 66, Impact Grade

PTEKNO419 / 128596

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.