MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chosun Refractories SAL50 Special Alumina brick
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.40 g/cc0.0867 lb/in³
Porosity 16 %16 %
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 58.8 MPa8530 psiCold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.00 µm/m-°C
@Temperature 1000 °C
2.78 µin/in-°F
@Temperature 1830 °F
Shrinkage -0.300 - 0.30 %
@Temperature 1600 °C,
Time 7200 sec
-0.300 - 0.30 %
@Temperature 2910 °F,
Time 2.00 hour
 
Component Elements PropertiesMetricEnglishComments
Al2O3 53 %53 %
Fe2O3 1.5 %1.5 %
 
Descriptive Properties
Main ApplicationLime Kiln, Cement Kiln, Various Rotary kiln, Reheating furnace, Glass melting Tank, Various furnace
Refractories Under Load(2kg/cm²,T2°C)1,550
Refractoriness (SK)36

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LKAB Minerals Mulcoa 70
China-Yixing Longly Refractories 75 Alumina Ceramic
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 60 PHR Dixie Clay Filler
MV Labs AL500 AlF3 Aluminum fluoride, anhydrous
Aluminum 5005-H32

CCHOS020 / 123964

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.