MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Geon® Performance Solutions 1100-xx22D Vinyl Compound - Wire & Cable  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes:

Description/Features:

  • UL Recognized Flexible Cord Wet-Location Insulation per UL QMTT2
  • UL Recognized 720 hr. Sunlight Resistant Jacket per UL QMTT2
  • UL 75°C
  • UL 60°C
  • STW
  • SJTW
  • SJT
  • SPT Cord
  • Flame Retardant

Applications:

  • Apparatus & Cord Jacket
  • Apparatus & Cord Insulation

Market:

  • Wire & Cable

Processing Method:

  • Extrusion Coating
PolyOne First Choice

Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Information provided by PolyOne Corporation.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 858515 sec; ASTM D2240
Tensile Strength, Yield 15.2 MPa2200 psiType 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break 290 %290 %Type 4 - Flexibles, 20 in/min; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.50e+12 ohm-cm5.50e+12 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -20.0 °C-4.00 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Melt Temperature 174 - 179 °C345 - 355 °FExtrusion
 
Descriptive Properties
Oven Aged - Retention of Elongation (ROE)95 %235°F (113°C), 168 hrs (7 days), 0.020 in; UL Standard
Oven Aged - Retention of Tensile Strength (ROT)100 %235°F (113°C), 168 hrs (7 days), 0.020 in; UL Standard
Product FormPellets/Cubes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PH1PO1124 / 43894

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.