MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Lehvoss LUVOCOM® NSB 90 BK-2 Nylon 66, PTFE Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, PTFE Filled

Material Notes: Polyamide 66 with PTFE, black

Main features: Improved friction and wear behavior. Optimized for dry running operations. Isotropic shrinkage characteristics.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccISO 1183-3
Water Absorption <= 1.00 %
@Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0150 - 0.0250 cm/cmDIN 16742
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 60.0 MPa50 mm/min; ISO 527
Elongation at Break 10.0 %50 mm/min, Fmax; ISO 527
Tensile Modulus 2.50 GPa1 mm/min; ISO 527
Flexural Strength 95.0 MPa10 mm/min; ISO 178
Flexural Modulus 2.90 GPa2 mm/min; ISO 178
Flexural Strain at Break 2.90 %10 mm/min, Fmax; ISO 178
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature -30.0 °C
80x10x4mm; ISO 179 1eU
 52.0 kJ/m²
@Temperature 23.0 °C
80x10x4mm; ISO 179 1eU
Charpy Impact, Notched 8.00 kJ/m²80x10x4mm; ISO 179 1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistance <= 1.00e+12 ohmRonde 60x4mm; DIN EN 62631-3-2
Insulation Resistance <= 1.00e+12 ohmstrip electrode R25; DIN EN 62631-3-3
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C10x8x4 mm; ISO 11359
Maximum Service Temperature, Air 100 °C
@Time 7.20e+7 sec
Continuous; IEC 60216
 140 °C
@Time 720000 sec
during lifetime
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C80x10x4mm; ISO 75
Vicat Softening Point 240 °CVST A; DIN ISO 306
Flammability, UL94 HB
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 280 - 300 °C
Zone 1 290 - 310 °C
Zone 2 290 - 310 °C
Zone 3 290 - 310 °C
Melt Temperature 290 °C
Mold Temperature 90.0 - 120 °C
Drying Temperature 75.0 °C
@Time 21600 - 57600 sec
Dehumidifying
 105 °C
@Time 14400 - 21600 sec
Vacuum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUU8718 / 325102

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.