MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dioshy VP-850 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: There are many soft and hard segment combinations of TPV (aka TPO-V). Very popular in American and European markets.

Features:

  • Possessed excellent heat resistance and elastic property, good chemical resistance, weather resistance and aging resistance.
  • Mostly applied for car parts.
  • Good anti-slip property, especially in wet status; very good compression set; white color and good coloring property; customized.
  • Suitable to dual color processing for PP or PE; also can be the toughener for PP or PE.
  • Suitable to mostly thermoplastic procedures; PVC replacement.
  • Green material, passed heavy metal regulation, RoHS and EACH –SVHC

    Information provided by DIOSHY CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.922 g/cc0.922 g/ccJIS-K6301
Melt Flow 3.48 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.48 g/10 min
@Load 4.76 lb,
Temperature 374 °F
JIS-K7210
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050JIS-K6301
Tensile Strength 3.82 MPa555 psiJIS-K6310
Elongation at Break 463 %463 %JIS-K6310
100% Modulus 1.18 MPa171 psiJIS-K6310
300% Modulus 0.883 MPa128 psiJIS-K6310
Tear Strength 202 kN/m1150 pliJIS-K6310-B
Compression Set 14 %
@Temperature 23.0 °C,
Time 79200 sec
14 %
@Temperature 73.4 °F,
Time 22.0 hour
JIS-K6301
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 155 - 165 °C311 - 329 °FInjection
 155 - 175 °C311 - 347 °FExtrusion
Middle Barrel Temperature 170 - 185 °C338 - 365 °FExtrusion
 175 - 185 °C347 - 365 °FInjection
Front Barrel Temperature 175 - 185 °C347 - 365 °FInjection
 175 - 190 °C347 - 374 °FExtrusion
Nozzle Temperature 195 - 205 °C383 - 401 °FInjection
Die Temperature 190 - 205 °C374 - 401 °FExtrusion
Drying Temperature 70.0 °C158 °F
Dry Time 1.00 hour1.00 hour
 
Descriptive Properties
Application Dual color processingPP
ColorWhite
TPS typeTPV-S

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDIOSH070 / 294680

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.