MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay CYCOM® 977-3 Epoxy - 5 Harness Satin (5HS) Carbon Fiber Prepreg
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: CYCOM® 977-3 is a 350°F (177°C) curing resin. It is a toughened epoxy resin with 350°F (177°C) dry and 270°F (132°C) wet service capability. CYCOM 977-3 is formulated for autoclave or press molding and can be cured at 350°F (177°C) for six hours. Unidirectional tape and woven fabric impregnated with CYCOM 977-3 resin will retain tack for 21 days at 72°F (22°C). It has a long mechanical out life suitable for fabrication of large structures.

Features & Benefits:

  • 350°F (177°C) cure
  • Available on fabric and tape
  • 350°F (177°C) dry service temperature
  • 270°F (132°C) wet service temperature
  • Laminate and sandwich panel usage
  • Autoclave or press mold processing
  • Toughened epoxy using proprietary “cocontinuous”morphology
  • Impact resistance
  • Shelf life of 12 months at 0°F (-18°C), 21 days at 72°F (22°C)
Applications:
  • Aircraft primary and secondary structure
  • Applications where impact resistance is critical
  • Applications where hot/wet performance is crucial
Mechanical property data for 977-3 epoxy with 5 Harness Satin (5HS) Standard Modulus Carbon Fiber 5HS AS4 6K [33 msi (228 GPa)].

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 122000 - 150000 psi
@Temperature 24.0 °C
Tensile Modulus 64.0 - 72.0 GPa
@Temperature 24.0 °C
90°
Shear Strength 11000 - 15000 psi
@Temperature 24.0 °C
0° Interlaminar
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 132 °Cwet
 177 °Cdry
Glass Transition Temp, Tg 178 °CG'
 189 °CG"
 190 °CTan Delta
 
Processing PropertiesOriginal ValueComments
Processing Temperature 350 °FCure
Shelf Life 0.630 Month
@Temperature 22.2 °C
 12.0 Month
@Temperature -17.8 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay CYCOM® 5320-1 Epoxy with T40/800B Unidirectional Tape Composite
Solvay CYCOM® 890 RTM Resin - Woven Carbon Fabric Composite
Solvay CYCOM® 5250-4 RTM BMI Resin, Composite with T650-35-3K-PW Fabric
Solvay CYCOM® 5250-4 RTM BMI Resin, Composite with IM7-6K-4HS Fabric
Solvay CYCOM® 977-3 Epoxy - Unidirectional Carbon Fiber Tape

PCYTED091a / 234746

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.