MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Polimersan Plastics POLITEF® (PTFE) with 15% Glass
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes:
  • Electrical Conductivity
  • Increase At Corrosion Resistance
  • Increase In Deformation Strength Against Load
  • Decrease In Thermal Expansion
  • High Resistance Against Acids
  • Ease of Mechanical Processing
  • Stretching
  • Resistance Against Stroke
  • Increase In Thermal Conductivity

Information provided by Polimersan Polimer Kimya San.Tic.Ltd.Sti.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.10 - 2.30 g/cc2.10 - 2.30 g/ccASTM D1457-18
Deformation 9.8 %9.8 %230°C, 1 day, 140 kg/cm^2; ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 57 - 6257 - 62ASTM D2240
Tensile Strength, Yield 21.6 - 23.5 MPa3130 - 3410 psiASTM D1708
Elongation at Break 290 - 300 %290 - 300 %ASTM D1708
Izod Impact, Notched 1.37 J/cm2.57 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 16.0 - 19.0 kV/mm406 - 483 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 - 140 µm/m-°C
@Temperature 20.0 °C
55.6 - 77.8 µin/in-°F
@Temperature 68.0 °F
ASTM E831
Thermal Conductivity 0.5577 W/m-K3.864 BTU-in/hr-ft²-°FASTM C177
 
Descriptive Properties
Corrosion15 - 25 cc-dak/kg-ms25 - 1000°C
Kinding Temperature630°C, ASTM D1929

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Murtfeldt Murflor® Polytetrafluoroethylene
Murtfeldt Murflor® Polytetrafluoroethylene, 25% Carbon
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Saint-Gobain Rulon® 1439 Bearing/Seal PTFE

PPOLIM01 / 56967

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.