MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Parker Chomerics Duralan™ G Glass Unshielded Window
Categories: Ceramic; Glass; Optical

Material Notes: Parker Chomerics glass windows are designed to offer substrates that provide the hardest surface for resistance to scratching and high temperature applications. These glass products are offered as a single sheet or as fully laminated windows, which closely match the properties of safety glass. There are various design options, such as a single layer, a full laminate or a step design depending on the customer’s design requirement.

Surface Finish Option: Anti-reflective and Anti-glare

Design Options: Screen Printing, Heat Shielding, Privacy Filters and Other Specific Applications Available

Typical Applications: Military, Aerospace, Medical, Industrial, Display Protection and Test Instrumentation

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 550 - 600 microns
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 1.0 %Reduction; Non-glare coatings (80-90 gloss)
 <= 1.0 %Clear hard coat
 <= 1.0 %MLAR coating on glass
 2.0 - 3.0 %Reduction; Non-glare coatings (60-70 gloss)
 83 - 88 %Clear polyester
 85 - 90 %Clear polycarbonate
 85 - 90 %Clear acrylic
 90 - 92 %Plane "float" glass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makroblend® UT-403 Polycarbonate + Polyester Blend
Corning Vycor® 7907 UV-Blocking Glass
Corning Vycor® 7904 Blue Glass
Corning Gorilla® Glass 2
Celanese WVC 3800 50000884 Plasticizer

PCHOME288 / 130998

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.