MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Elvaloy® AC 2618 Ethylene Methyl Acrylate
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Extrusion Grade

Material Notes: Elvaloy® AC 2618 is a copolymer of ethylene and ethyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins.

Elvaloy® AC 2618 resin complies with the U. S. Food and Drug Administration regulation 21 CFR177.1320; Ethylene Ethyl Acrylate copolymers, for use in contact with food, except for holding food during cooking. These EEA resins must be blended with olefin polymers complying with 21 CFR 177.1520 in such proportions that the ethyl acrylate content of the blend does not exceed 8 percent by weight. Migration limits must also be complied as specified in paragraph (c)(2).

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D792, ISO 1183
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238, ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 95.0 °CASTM D3418, ISO 3146
Vicat Softening Point 56.0 °CASTM D1525, ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 310 °C
Feed Temperature 185 °CExtrusion Coating
Zone 2 235 °CExtrusion Coating
Zone 3 260 °CExtrusion Coating
Zone 4 285 °CExtrusion Coating
Zone 5 285 °CExtrusion Coating
Adapter Temperature 285 °CExtrusion Coating
Die Temperature 285 °CExtrusion Coating
Melt Temperature 235 - 310 °CExtrusion Coating
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Elvaloy® AC 1330 Ethylene Methyl Acrylate
Dow Elvaloy® 741WR Ethylene/Vinyl Acetate/Carbon Monoxide (E/VA/CO) Copolymer
Dow Elvaloy® AC 12024S Ethylene Methyl Acrylate
Dow Elvaloy® AC 15024S Ethylene Methyl Acrylate
Dow Elvaloy® AC34035 Ethylene Methyl Acrylate

PDTA4938 / 170378

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.