MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Johnson Matthey Silver-flo™ 252 Cadmium Free Silver Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Solder/Braze Alloy

Material Notes: Silver-flo™ 252 is a cadmium-free silver brazing filler metal. It has a medium melting temperature (680 to 760°C) with a long melting range of 80°C. This melting range suggests that Silver-flo™ 252 will demonstrate medium to sluggish flow and good gap filling properties when molten. This makes it an ideal choice for applications where fillets are required or close tolerance joint gaps are not present.

With a fast heating method Silver-flo™ 252 may be used below the point at which it becomes necessary to use a high temperature flux enabling easier removal of flux residues after brazing.

Optimum joint gaps at brazing temperature are 0.075-0.2mm.

Silver-flo™ 252 can be used to join most common engineering metals - copper, copper alloys including, brasses, bronzes, gun metal, nickel silver, aluminum bronze, copper nickel, steels including, mild, carbon, tool steel, stainless steels, low alloy steel. This alloy is not normally recommended for brazing tungsten carbide and PCD segments where lower melting or nickel / manganese containing silver brazing filler metals are often preferred.

Silver-flo™ 252 may be used for brazing steel to steel and copper to steel pipe work in the refrigeration, heat exchanger and air-conditioning industries for example.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 680 - 760 °C
Solidus 680 °C
Liquidus 760 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 40 %
Silver, Ag 25 %
Tin, Sn 2.0 %
Zinc, Zn 33 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NJMMJ9778 / 186179

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.