MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC Fluon® FR 22 PTFE, 10% Graphite Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: Fluon® FR 22 (330 022 001) is a 10% graphite powder-filled PTFE product designed for use in seal applications. This compound is supplied in round pelletized form. These pellets range in size from approximately 350 – 800 microns.

End Uses: Graphite powder is added to PTFE to improve the lubricity and wear properties of PTFE especially against soft metals.

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.14 g/cc2.14 g/ccASTM D4745
Bulk Density 0.775 g/cc0.0280 lb/in³ASTM D4894
Filler Content 10 %10 %ASTM D4745
Linear Mold Shrinkage 0.022 cm/cm0.022 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 19.3 MPa2800 psiASTM D4745
Elongation at Break 200 %200 %ASTM D4745

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC Fluon® FP-EF-101 PTFE, 5% Glass Filled
AGC Fluon® FC168-63 PTFE, 63% Bronze and Graphite Filled
AGC Fluon® FC123 PTFE, 15% Graphite Filled
AGC Fluon® FC100-25 1000 PTFE, 25% Glass Fiber Filled
AGC Fluon® FC100-15 1000 PTFE, 15% Glass Fiber Filled

PAGCX132 / 191241

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.