Available Forms: Flat Sheets Masking: Other Properties: Flame Retardant Optical Properties: Transparent; UV Stabilized Surface: Smooth Weatherability: Indoor Sizes: 49” x 79” Thicknesses: 0.060”; 0.080”; 0.125”; 0.157”; 0.197” Applications: Aircraft GlazingInformation provided by Roehm America LLC |