MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röchling SUSTARIN® C ESD 60 PLUS POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Product characteristics:
  • Electrically conductive
  • Very high stiffness
  • High dimensional stability
Product applications:
  • Mechanical engineering
  • Explosion protection
  • Conveyor technology

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³DIN EN ISO 1183-1
Water Absorption 0.20 %0.20 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7878DIN EN ISO 868
Ball Indentation Hardness 180 MPa26100 psiDIN EN ISO 2039-1
Tensile Strength, Yield 45.0 MPa6530 psiDIN EN ISO 527
Elongation at Break 10 %10 %DIN EN ISO 527
Modulus of Elasticity 3.70 GPa537 ksiDIN EN ISO 527
Izod Impact, Notched (ISO) 2.50 kJ/m²1.19 ft-lb/in²DIN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 10000 ohm<= 10000 ohmDIN EN 62631-3-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FISO 11357-3
Maximum Service Temperature, Air 100 °C212 °Flong term
 140 °C284 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FDIN EN ISO 75
Minimum Service Temperature, Air -20.0 °C-4.00 °F
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 HB
@Thickness 6.00 mm
HB
@Thickness 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röchling SUSTARIN® H AF - DE588 POM/Acetal Homopolymer
RTP Company RTP 801 CC  Acetal (POM) Chemically Coupled - Glass Fiber 10%
Polyram RamTal PMH2022 Polyacetal Homopolymer for Injection Molding
Murtfeldt Murytal® H Acetal Homopolymer
Mitsubishi Iupital® TC3015 Copolymer Acetal

PROCH9338 / 233040

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.