MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Innegra™ Techologies Innegra™ S IS-1880 Olefinic Fiber
Categories: Other Engineering Material; Composite Fibers; Polymer

Material Notes: Innegra S is an olefin based high performance yarn used most often in conjunction with a high modulus fiber to increase toughness, durability, dampening, and in some cases, reduce weight.

When high modulus fibers are combined with Innegra™ S fiber, weight can be reduced, impact resistance, damage tolerance and signal transmission vastly improved, expanding the performance of existing materials. Properties of Innegra™S Fiber include:

  • Multi-filament, high modulus olefin yarn
  • Hydrophobic
  • Tough
  • Ductile
  • Durable
  • Low Dielectric Properties
  • Low Elongation
  • Low Creep
  • Highly Crystalline
  • Recyclable
Available in white or black

Preliminary property data is reported.

Information provided by Innegra Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.840 g/cc
Fiber Count 1880 denierASTM D1907
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 667 MPaUsing density of 0.84 g/cc; ASTM D885
Elongation at Break 10 %ASTM D885
Tensile Modulus 14086 MPaUsing density of 0.84 g/cc; ASTM D885
Tenacity 9.00 g/denierASTM D885
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.2
Dielectric Loss Index 0.00090
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °CDSC; Processing/Service Limit
 
Descriptive Properties
Breaking Strength37.3 lbF (16.9 kgF)ASTM D885
Creep (%)3.21 year; RT; 20% UTS
Filaments per tow150
Yield2375 yd/lb4787 m/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexTow® IM6 Carbon Fiber - Epoxy Composite
DuPont™ Nomex® 414 Paper, 10 mil Nominal Thickness
Beijing Evergrow Resources BF-25 Basalt Needle Felt
Mid-Mountain Materials HYTEX® 700 Kevlar® Glass Industrial Textile
Mid-Mountain Materials HYTEX® 500 Nomex® Industrial Textile

PINNEG903 / 179543

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.