MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ExxonMobil EXACT™ 4042 Plastomer for Polymer Modification  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyethylene (PE)

Material Notes: Data provided by the manufacturer, Exxon Chemical.

An ethylene-based plastomer produced using Exxon Chemical's EXXPOL technology, exhibiting both plastic and elastomeric properties. This resin is designed for modification of both polypropylenes and polyethylenes in applications such as injection molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.899 g/cc0.0325 lb/in³Exxon Method
Mooney Viscosity 19
@Temperature 125 °C
19
@Temperature 257 °F
Torque Units, Mooney Viscosity (1+4); ASTM D-1646
Environmental Stress Crack Resistance >= 1000 hour>= 1000 hourF50, Condition A; ASTM D1693
Melt Flow 1.7 g/10 min1.7 g/10 minExxon Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9393ASTM D2240
Hardness, Shore D 4040ASTM D2240
Tensile Strength, Ultimate 57.0 MPa8270 psiASTM D638
Tensile Strength, Yield 7.60 MPa1100 psiASTM D638
Elongation at Break 750 %750 %ASTM D638
Elongation at Yield 190 %190 %ASTM D638
Flexural Modulus 0.0610 GPa8.85 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
Instrumented Impact Total Energy 45.0 J
@Temperature 23.0 °C
33.2 ft-lb
@Temperature 73.4 °F
ASTM D-4272
Tear Strength 95.0 kN/m542 pliDie C; ASTM D-624
 
Thermal PropertiesMetricEnglishComments
Melting Point 92.0 °C198 °FExxon Method
Vicat Softening Point 81.0 °C178 °F1000g; ASTM D-1525
 
Optical PropertiesMetricEnglishComments
Haze 8.0 %8.0 %ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEXCIO / 38044

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.