MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Polymist® F5A Polytetrafluoroethylene (PTFE) Powder  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Polymist® F5A a white PTFE micronized powder PTFE micronized powder composed of discrete particles.

Designed for use in critical engineering and high-end performance elastomers and coatings, Polymist® F5A will improved abrasion and tear resistance as well as non-stick properties, mar and abrasion resistance.

Polymist® F5A can also be used in plastics application to improved wear resistance and low coefficient of friction or in lubricants for its thickening effect, lubricity, improved corrosion and temperature resistance.

Main features of Polymist® F5A are:
- Improved lubricity, abrasion, scratch and rub resistance
- Increased (hot) tear strength
- Better flex life
- Increased slip and surface lubricity
- Reduced blocking
- Better chemical resistance
- Increased temperature resistance
- Gloss retention

Applications: Additive

Processing
- Besides its main function as a wear additive, Polymist® F5A can be used at low concentration to improve mold release properties.
- Internal or open mixers (e.g. Banbury or two-roll mixers) are normally used to allow a good distribution of Polymist® F5A in the elastomeric compound. Additional fillers are normally included with Polymist micronized PTFE during the blending process. The resulting elastomeric composition can then be processed under normal conditions.
- Polymist® F5A can also be used as additives in paints and coatings where improvements in non-stick, mar resistance, slip, chemical resistance, and moisture repelling characteristics are desired. Polymist® F5A may be used independently as an additive or in combination with polyethylene waxes. The PTFE content at the surface layer is required in order to impart the properties of PTFE to the coating.

Storage and Handling
- The usual precautions for safe storage and handling of Polymist® F5A should be taken according to material safety documentation and experience. There will be no chemical deterioration of the Polymist® F5A during proper storage.
- Shelf life of Polymist® F5A micronized powders will vary depending upon whether the recommended storage conditions are maintained and whether the material remains free from foreign contamination during storage time (not exposed to dirt, dust, water or other chemicals). The material should remain sealed in the original containers and storage conditions should provide for protection from temperature extremes as well as rain, snow or other wet environments (or such conditions which may damage the storage containers in which the product is stored).

Safety and Toxicology
- Before using Polymist® F5A PTFE micronized powders, consult the product Material Safety Data Sheet and follow all label directions and handling precautions.
- As with all PTFE materials, handling and processing should only be carried out in well ventilated areas. Vapor extractor units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact wash with soap and water. In case of eye contact flush with water immediately and seek medical help.
- Do not smoke in areas contaminated with powder, vapor or fumes.
- See Material Safety Data Sheet for detailed advice on waste disposal methods.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.400 g/ccASTM D4895
Particle Size 4.0 - 15 µmAverage; Internal Method
 
Descriptive Properties
Availability (as of March 2019)Asia Pacific; Europe; North America
ColorWhite
FormsPowder

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Phillips 66 Dynalife® HT NLGI Grade 2
General Plastics LAST-A-FOAM® R-9320 Thermal Isolation Blocks
Dover Chemical EM 995 Fatty Amide Lubricity / Corrosion Inhibitor

PSOL8Y5261 / 238642

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.