MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Westlake Plastics Tempalux® CN-F Polyetherimide (conductive)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Non-sloughing carbon-fiber filled material which is extremely strong and stiff, has excellent dimensional stability, and high temperature resistance to 415F. This material has broad chemical resistance and excellent fabrication finishing characteristics. UL94 V-0 rated.

Information provided by Westlake Plastics.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ASTM D792
Water Absorption 0.45 %0.45 %ASTM D570; 24 hrs.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9292ASTM D2240
Tensile Strength, Yield 200 MPa29000 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Flexural Strength 262 MPa38000 psiASTM D790
Flexural Modulus 12.8 GPa1860 ksiASTM D790
Izod Impact, Notched 0.747 J/cm1.40 ft-lb/inASTM D256
Izod Impact, Unnotched 4.00 J/cm7.50 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10000 ohm-cm - 1e+0510000 ohm-cm - 1e+05Dry; ASTM D257
Surface Resistance 10000 ohm - 1e+0510000 ohm - 1e+05Dry; ASTM D257
Static Decay <= 0.10 sec<= 0.10 sec15% RH; MIL-B-81705-B
 
Thermal PropertiesMetricEnglishComments
CTE, linear 39.6 µm/m-°C
@Temperature 20.0 °C
22.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 214 °C417 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.47 mm
V-0
@Thickness 0.0580 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Semitron™ MP-370 Polyphenylsulfone
Westlake Plastics Tempalux® Film Made from ULTEM® Polyetherimide Resin
Mitsubishi Chemical Advanced Materials Semitron™ MDS 100 PEEK
Mitsubishi Chemical Advanced Materials Semitron™ ESd 490HR PEEK Non-sloughing and low moisture absorption
Mitsubishi Chemical Advanced Materials Semitron™ ESd 480 PEEK, static dissipative

PWEST051 / 72731

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.