MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Cabot MONARCH® 1000 Specialty Carbon Black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product highlights: MONARCH® 1000 specialty carbon black is a small particle treated grade designed to enable excellent jet masstone with strong tinting strength in high performance automotive, industrial and architectural coatings.

Key applications: MONARCH 1000 specialty carbon black has small particles that enable excellent jetness and UV absorption for good exterior durability. It is suitable for use in high-end coatings that require high jetness and strong tinting strength.
Coatings: MONARCH 1000 specialty carbon black is suitable for use in liquid, automotive, industrial and architectural coatings. The dispersibility of this product is enhanced by its high structure and surface treatment. The degree of dispersion will depend on the equipment used and the formulation. A product with similar morphology, BLACK PEARLS® 1000 specialty carbon black, is available in an easier-to-handle pelleted form.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 9.0 %9.0 %CTM 16.1
Ash <= 0.50 %<= 0.50 %ASTM D-1506
 
Descriptive Properties
Iodine absorption520 mg/gCTM 23.4, Devolatilized
OAN110 cc/100gASTM D-2414
Product Formfluffy

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT169 / 315904

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.