MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron AboCast/AboCure 8110-2 Flexible Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive, Flexible

Material Notes: This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applications include: bonding, laminating, casting, embedding, electrical potting, impregnating, coating, etc. It can be supplied in several variations to modify viscosity, reaction rate, color, most physical and chemical properties, and with many fillers to meet most requirements.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 3.3 %
@Time 2.59e+6 sec
immersion; cured 7 days @ 25°C
 3.3 %
@Time 2.59e+6 sec
immersion; cured 30 days @ 25°C
Viscosity 2260 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 33
@Temperature 75.0 °C
cured 7 days @ 25°C
 42
@Temperature 75.0 °C
cured 30 days @ 25°C
 82
@Temperature 25.0 °C
cured 7 days @ 25°C
 84
@Temperature 25.0 °C
cured 30 days @ 25°C
 86
@Temperature 0.000 °C
cured 30 days @ 25°C
 87
@Temperature 0.000 °C
cured 7 days @ 25°C
 89
@Temperature -60.0 °C
cured 7 days @ 25°C
 89
@Temperature -60.0 °C
cured 30 days @ 25°C
Tensile Strength, Ultimate 6625 psicured 7 days @ 25°C
 7050 psicured 30 days @ 25°C
Elongation at Break 12 %cured 30 days @ 25°C
 20 %cured 7 days @ 25°C
Shear Strength 370 psi
@Temperature 75.0 °C
Tensile, Al/Al lap joint; cured 7 days @ 25°C
 3950 psi
@Temperature 25.0 °C
Tensile, Al/Al lap joint; cured 7 days @ 25°C
 4400 psi
@Temperature 0.000 °C
Tensile, Al/Al lap joint; cured 7 days @ 25°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.60e+9 ohm-cm
@Temperature 100 °C
cured 30 days @ 25°C
 1.70e+10 ohm-cm
@Temperature 100 °C
cured 7 days @ 25°C
 3.30e+14 ohm-cm
@Temperature 25.0 °C
cured 30 days @ 25°C
 7.10e+14 ohm-cm
@Temperature 25.0 °C
cured 7 days @ 25°C
 
Processing PropertiesOriginal ValueComments
Pot Life 40 min
@Temperature 25.0 °C
200 g
 
Descriptive Properties
Parts by Weight (pbw)100AboCast 8110-2
 16.5AboCure 8110-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bakelite® PF 31 Phenolic Formaldehyde Resin, UL Listed
Resinoid 7201 Phenolic Molding, Glass Reinforced
Bakelite® PF 85 Phenolic Formaldehyde Resin, UL Listed
Bakelite® PF 4041 Phenolic Formaldehyde Resin, Resistant to High Temperatures
Abatron AboJet Structural Crack-Injection Resin

PABC868 / 107852

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.