Data provided by Solvay Engineered Polymers. A thermoplastic olefinic elastomer (TPO) designed for exterior automotive applications requiring excellent low-temperature toughness and flex-fatigue properties. Uses: Air dams and other semi-flexible components. LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line. |
Thermoplastic Olefinic Elastomer; Polyolefin |