MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Microthene® G MN71120 Low Density Polyethylene (Rotomolding)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes:

General Description
Microthene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique properties of a polyolefin resin with a small ground particle size.

Process Techniques
The microfine size and irregular shape of Microthene G powders facilitate dispersibility with other components. Specific suggestions can be made only when equipment, materials, process parameters and conditions of use are known.

Regulatory Status
Microthene powders comply with certain Food and Drug Administration regulations, which may or may not permit their contact with food. Specific limitations or conditions of use may apply.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.915 g/ccASTM D1505
Particle Mesh Size 35 MeshIrregular shape. ETM = Equistar Test Method; ETM Sieve Analysis
Melt Flow 22 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 52ASTM D2240
Tensile Strength at Break 1600 psiASTM D638
Elongation at Break 550 %ASTM D638
Flexural Modulus 17600 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 104 °CASTM D3418
Vicat Softening Point 83.0 °CASTM D1525
Brittleness Temperature -56.0 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil LLP8555.25 Rotational Molding Resin
NOVA Chemicals SURPASS® RMs539-U sLLDPE Rotational Molding Resin
LyondellBasell Petrothene® NA247000 Low Density Polyethylene, Injection Molding Grade
LyondellBasell Lupolen 3621 M RM Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
LyondellBasell Purell PE1840H Low Density Polyethylene, Blown Film, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding

PEQU0243 / 36677

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.