MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

UBE UBEPOL BR® 133P Synthetic Polybutadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Characteristics: Paraffinic oil extended grade. Oil content : 37.5phr. Superior low temperature properties. Suitable for high loading of filler. Applications: Tires for passenger cars, trucks, buses, construction machinery, motorcycles and bicycles. Various industrial products such as polystyrene modifier, conveyor belts, hoses, rubber isolators and casters. Commodities such as shoe soles and golf balls.

Polybutadiene rubber (BR) is one of typical rubbers and polymerized with a cobalt catalyst. UBE’s proprietary process technologies makes it is easy to control the molecular weight, the degree of branching of molecular chains and molecular weight distribution of the BR.

Information provided by UBE Industries, LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 g/cc0.890 g/cc
Mooney Viscosity 35
@Temperature 100 °C
35
@Temperature 212 °F
ML1+4
 
Descriptive Properties
Anti-OxidantNon-staining
Microstructure1Trans. % wt. Microstructure of matrix polymer.
 1Vinyl. % wt. Microstructure of matrix polymer.
 98Cis. %wt. Microstructure of matrix polymer.
Oil Content37.5phr
Package35 kg bale

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PUBD9802 / 287265

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.