MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Total Corbion Luminy LX130U PLA, Biobased Polymer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Luminy LX130U is a medium viscosity, medium flow, amorphous, transparent PLA resin suitable for injection molding and fiber spinning.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³Literature Value
Melt Flow  7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-A
 14 g/10 min
@Load 2.16 kg,
Temperature 210 °C
14 g/10 min
@Load 4.76 lb,
Temperature 410 °F
ISO 1133-A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 45.0 MPa6530 psiISO 527-1
Elongation at Break <= 5.0 %<= 5.0 %ISO 527-1
Tensile Modulus 3.50 GPa508 ksiISO 527-1
Charpy Impact Unnotched <= 0.500 J/cm²
@Temperature 23.0 °C
<= 2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 145 - 160 °C293 - 320 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 55.0 - 60.0 °C131 - 140 °FAmorphous; ISO 75-1
Glass Transition Temp, Tg 55.0 - 60.0 °C131 - 140 °FDSC
 
Processing PropertiesMetricEnglishComments
Feed Temperature 155 - 175 °C311 - 347 °F
Nozzle Temperature 180 - 220 °C356 - 428 °F
Mold Temperature 90.0 - 100 °C194 - 212 °F
Dry Time 4.00 - 6.00 hour
@Temperature 100 °C
4.00 - 6.00 hour
@Temperature 212 °F
Moisture Content <= 0.040 %<= 0.040 %Coulometric Karl-Fischer
Back Pressure 5.00 - 10.0 MPa725 - 1450 psi
 
Descriptive Properties
Residual Monomer<0.3%Total Corbion PLA Method
Stereochemical Purity96% (L-isomer)Total Corbion PLA Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NatureWorks® Ingeo™ 3801X Injection Grade PLA
Overview of materials for Polylactic Acid (PLA) Biopolymer
Total Corbion Luminy L130 PLA, Biobased Polymer
Total Corbion Luminy LX175 PLA, Biobased Polymer
Unitika TERRAMAC TE-1030 Polylactic Acid (PLA)

PTOTAC006 / 209624

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.