MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Rogers Arlon CP-594CX Bulk Compound
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Product Use: Electrically insulating electronic adhesive. Bonds without primer.

Appearance: Gray, high viscosity gum

UL94V-0: The product is designed to meet UL94V-0 flame resistance requirements but is not recognized by Underwriters Laboratories.

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.80 g/ccSilicone Property; Arlon SQA-TMS-024
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 77Silicone Property; ASTM D2240
Tensile Strength 685 psiSilicone Property; ASTM D412
Tensile Strength, Yield 3.55 ksi
@Strain <=1 %
Silicone Property; Arlon-SAQ-TMS-008
Elongation at Break 125 %Silicone Property; ASTM D412
Poissons Ratio 0.50Approximately, Silicone Property
Shear Modulus 0.00817 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 6.9
@Frequency 1e+6 Hz
Dk, Silicone Property; IPC TM 650-2.5.5.3
Dissipation Factor 0.0044
@Frequency 1e+6 Hz
Df, Silicone Property; IPC TM 650-2.5.5.3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 111 µm/m-°C
@Temperature 20.0 - 160 °C
Silicone Property; ASTM E 831
Specific Heat Capacity 0.820 J/g-°C
@Temperature 100 °C
Silicone Property; E1461-01
Thermal Conductivity 1.40 W/m-K
@Temperature 100 °C
Silicone Property; ASTM E 1530
Maximum Service Temperature, Air 399.2 °F
Minimum Service Temperature, Air -148 °F
Glass Transition Temp, Tg -118 °CSilicone Property; ASTM D3418
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Pressure 0.101 - 0.345 MPa,
Temperature 121.0 °C
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature 7.00 °C
From date of manufacture
 
Descriptive Properties
ColorGray
Plasticity2.3 mmArlon SQA-TMS-005

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber
A. Schulman BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound
Covestro Baybond® PU 406 Polyurethane
Covestro Baybond® PU 330 Polyester Urethane Polymer
CHT Group SMP™ EP 1009 EPI Engineered Polymers Silicone Modified Polymer

PARL520 / 125706

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.