MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Invista 1101R Copolymer Packaging Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Carboxyl end groups: <35 meg/kg.
Diethylene glycol content: <1.8 wt%.
Acetaldehyde content: <2.0 ppm.
Fines 0.05% through 28 mesh as manufactured.
Moisture content <0.1% as manufactured.
Chip size <2.0 g/100 chips.
Crystallinity > 50%.

1101R PET is a copolymer packaging resin with a nominal intrinsic viscosity of 0.83 dl/g.

Packaging made from this resin has excellent clarity and is noted for its dimensional stability, which prevents shrinkage and expansion of the container. 1101R is used successfully in carbonated soft drink bottles and other applications such as food containers and packaging for household goods. This resin complies with the Federal Food, Drug, and Cosmetic Act for certain food contact applications.

1101R offers excellent performance in maximum throughput, stretch-blow molding applications. Preforms made from 1101R allow maximum blowing throughputs by quickly heating the infrared (IR) ovens. In addition, bottles made from 1101R are low-stick, which eases handling issues.

Containers made from PET are lightweight, have excellent clarity, and are shatterproof. With the important advantage of being totally recyclable, PET is becoming the packaging resin of choice.

Information from manufacturer data sheet.

The Invista PET product line has been acquired by Indorama.

Key Words: Excellent melt and crystallization properties
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density >= 0.830 g/ccPycnometer test
Density >= 1.39 g/ccPycnometer test
Viscosity 0.81 - 0.85 cPIntrinsic viscosity; WI No. 104 test; correlated from solution viscosity by Invista
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 252 °CDSC test
 
Descriptive Properties
ProcessBlow Molding
 Injection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Invista 2201U Copolymer Packaging Resin
Eastman Eastar GN078 Copolyester, Natural
Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film
Kolon CGP21 Corona Metallized Packaging Film
Michelman® Michem® Tite 242AF Skin packaging primer

PKO010 / 48898

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.