MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Elastomer Engineering Elastamide 100 Elastomer Modified RIM Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: 30% crystallinity. Information supplied by Elastomer Engineering.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 3.1 %3.1 %24 hrs; DIN 53714
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7474
Tensile Strength, Ultimate 49.0 MPa7110 psiASTM D638
Elongation at Break 250 %250 %ASTM D638
Tensile Modulus 1.20 GPa174 ksiASTM D638
Flexural Modulus 1.17 GPa170 ksiASTM D790
Izod Impact, Notched 3.52 J/cm6.59 ft-lb/inMethod B; Ductile Failure
 0.430 J/cm
@Temperature -40.0 °C
0.806 ft-lb/in
@Temperature -40.0 °F
Method B; Brittle Failure
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²Brittle Failure; ASTM D256B
 0.310 J/cm²
@Temperature -40.0 °C
1.48 ft-lb/in²
@Temperature -40.0 °F
Method B; Brittle Failure
Taber Abrasion, mg/1000 Cycles 1010
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  4.1
@Frequency 100000 Hz
4.1
@Frequency 100000 Hz
 7.9
@Frequency 1000 Hz
7.9
@Frequency 1000 Hz
 15.3
@Frequency 50 Hz
15.3
@Frequency 50 Hz
Dielectric Strength 13.0 kV/mm330 kV/in
Dissipation Factor  0.10
@Frequency 100000 Hz
0.10
@Frequency 100000 Hz
ASTM D150
 0.30
@Frequency 1000 Hz
0.30
@Frequency 1000 Hz
ASTM D150
Comparative Tracking Index 400 V400 VASTM D257

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Brueggemann Chemical Nyrim® 1000 (Dry)
DSM Fibre Intermediates Nyrim® 1500 (Dry)
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 20 pcf, MDI-based 2-Component Liquid System
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 30 pcf, MDI-based 2-Component Liquid System
Covestro Baydur® GS-772 Polyurethane Solid RIM, MDI-based 2-Component Liquid System

PELA00 / 35667

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.