MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

En-Door ED-G32 PVC Internal Lubricant
Categories: Other Engineering Material

Material Notes: General Information: ED-G32 is compound fat alcohol ester that the long chain fatty acid complex with fatty alcohol ester. It can improve mobility and prevent adherence during processing. Incompatible with lead stabilizer.

Application: It is widely used in rigid and soft PVC production and plasticization. Applied in non-transparent products. The Recommended dosage is 0.5-1.5phr for rigid/soft PVC products, 0.05-2.0phr for PVC plasticization process, 1.6-2.0 phr for rigid PVC plate.

Information provided by En-Door

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 2.0 %
@Temperature 105 °C,
Time 7200 sec
<= 2.0 %
@Temperature 221 °F,
Time 2.00 hour
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 5.0<= 5.0[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Melting Point 54.0 - 58.0 °C129 - 136 °F
Flash Point >= 240 °C>= 464 °F
 
Descriptive Properties
AppearanceWhite or yellowish liquid
Iodine value<4gI2/100g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENDOOR038 / 316672

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.