LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical, fracture-sensitive aerospace structural applications. It is double vacuum melted (VIM-VAR…vacuum induction melted followed by vacuum arc remelting) to provide superior
cleanliness, ingot homogeneity, and to enhance mechanical properties. Heat Treatment - 857°C - 1 hour oil quench; -73°C - 1 hr air warm; 510°C - 5 hrs air cool Information Provided by Timken Latrobe Steel. Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co. |