MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAKEEP® 2000G PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: VESTAKEEP 2000G is a medium-viscosity, unreinforced polyether ether ketone for injection molding. The semi-crystalline polymer features superior thermal and chemical resistance. Parts made from VESTAKEEP 2000G are self-extinguishing. VESTAKEEP 2000G can be processed by common injection molding machines for thermoplastics.

Information provided by Evonik

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0011 cm/cmdetermined on 2 mm sheets with film gate at rim mold temperature 180°C; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0011 cm/cmdetermined on 2 mm sheets with film gate at rim mold temperature 180°C; ISO 294-4
Melt Flow 70 g/10 min
@Load 5.00 kg,
Temperature 380 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 100 MPaISO 527-1
Elongation at Break 30 %ISO 527-1
Elongation at Yield 5.0 %ISO 527-1
Tensile Modulus 3700 MPaISO 527-1
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 2.8
@Frequency 50 Hz
IEC 60250
 2.8
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 16.0 kV/mmIEC 60243-1
Comparative Tracking Index 175 V100 drops value; IEC 60112
 200 VCTI; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359
Melting Point 340 °CISO 11357
Vicat Softening Point 310 °C
@Load 5.10 kg
Method B; ISO 306
 335 °C
@Load 1.02 kg
Method A; ISO 306
Flammability, UL94 V-0
@Thickness 3.20 mm
IEC60695
Glow Wire Ignition Temperature 800 °C
@Thickness 2.00 mm
IEC 60695-2
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
IEC 60695-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 360 - 380 °C
Mold Temperature 160 - 200 °C
 180 °CPreferred

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone
Evonik VESTAKEEP® 4000G PEEK
Evonik VESTAKEEP® M4G PEEK
Evonik VESTAKEEP® 1000P PEEK
Evonik VESTAKEEP® 4000P PEEK

PEVONIL208 / 196412

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.