MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik VESTAMID® LX9013 BK 9.7507 Nylon 12, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® LX9013 BK 9.7507 is a plasticized polyamide 12 compound with an especially high long-term resistance under thermal load. The material absorbs only little moisture, thus leading to nearly unaffected dimensions and properties of the finished parts at changing ambient conditions. Extruded tubes are impact-resistant also at low temperatures. VESTAMID® LX9013 BK 9.7507 is suited to produce flexible tubes that are permanently exposed to higher temperatures, e.g., in the engine compartment of motor vehicles. Especially when used as diesel fuel lines they show significant advantages compared with standard grades, obvious in storage tests with diesel fuel (see the figure). The material corresponds to the extrusion compound PA12-HIPHL, grade1 acc. DIN 73378 and meets the requirements acc. DIN 74324 (black), ISO 7628 and SAE J844. VESTAMID® LX9013 BK 9.7507 is supplied as pellets in moisture-proof packaging ready for processing. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C
Industrial Sector: Automotive and Mobility, Sustainable
Sustainability: Sustainable electricity
Processing: Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels
Electrical: Insulating
Conformity: Automotive
Additives: Unfilled
Applications: Tube and hose
Processing: Profile extrusion, Pipe/Tube extrusion
Special Characteristics: High impact strength, High heat resistant, High viscosity
Color: Black
Additives: Plasticizer, Impact restistant, Heat stabilizer
Delivery form: Fuel resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 69.0
@Time 3.00 sec
69.0
@Time 0.000833 hour
ISO 7619-1
Tensile Strength at Break 41.0 MPa5950 psiISO 527
Elongation at Break 150 %150 %Nominal; ISO 527
Tensile Modulus 0.400 GPa58.0 ksiISO 527
Flexural Strength 15.0 MPa2180 psiISO 178
 27.0 MPa3920 psiISO 178
Flexural Modulus 0.440 GPa63.8 ksiISO 178
Flexural Strain at Break 10.0 %10.0 %at flexural strength; ISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 14.0 J/cm²
@Temperature 23.0 °C
66.6 ft-lb/in²
@Temperature 73.4 °F
Type of failure: P; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.10e+7 ohm-cm5.10e+7 ohm-cmIEC 62631-3-1
Surface Resistance 1.50e+12 ohm1.50e+12 ohmcircular electrodes; IEC 62631-3-2
Dielectric Constant  3.60
@Frequency 1.00e+6 Hz
3.60
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 15.6
@Frequency 100 Hz
15.6
@Frequency 100 Hz
IEC 62631-2-1
 18.4
@Frequency 50.0 Hz
18.4
@Frequency 50.0 Hz
IEC 62631-2-1
Dielectric Strength 23.0 kV/mm584 kV/inAC, S20/S20, t.; IEC 60243-1
Dissipation Factor  0.139
@Frequency 1.00e+6 Hz
0.139
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 0.665
@Frequency 100 Hz
0.665
@Frequency 100 Hz
IEC 62631-2-1
 
Descriptive Properties
Blue water consumption25.9 kgISO 14040, 14044
ColorBlack
Flexural stress at breakNMPa, ISO 178
 N%, ISO 178
Global Warming Potential2.6 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 5.7 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
 5.8 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.3 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7923 / 325055

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.