MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt CDA 681 Low Fuming Bronze Filler Metal
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy

Material Notes: CDA 681 is a low fuming bronze filler metal used for brazing of ferrous and non-ferrous alloys such steel and copper. This alloy is typically used where close fit up cannot be maintained and high brazing temperatures are permissible. CDA 681 has a good wetting characteristics on ferrous and non-ferrous materials particularly steels and coppers.

Available forms: Wire, strip, engineered preforms, specialty preforms, powder and paste.

Information provided by Lucas-Milhaupt.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 8.07 g/cc
Density 0.292 lb/in³
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000718 ohm-cm24% IACS
 
Thermal PropertiesOriginal ValueComments
Melting Point 1590 - 1630 °F
Solidus 1590 °F
Liquidus 1630 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1670 - 1750 °FBrazing Range
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.010 %
Copper, Cu 56 - 60 %
Iron, Fe 0.30 - 1.2 %
Lead, Pb 0.050 %
Manganese, Mn 0.010 - 0.50 %
Other, total <= 0.50 %
Silicon, Si 0.040 - 0.15 %
Tin, Sn 0.80 - 1.1 %
Zinc, Zn 36.5 - 42.3 %Remainder
 
Descriptive Properties
ColorBrass Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NLUCM9866 / 254799

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.