MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Matexcel MET-0020 Titanium-based TA15 Powder
Categories: Metal; Nonferrous Metal; Titanium Alloy

Material Notes:

Application: The high strength-to-weight ratio and outstanding corrosion resistance inherent, excellent biocompatibility of Titanium and its alloys have led to a wide range of successful applications in aerospace, automotive, power generation, chemical plant, sports, oil and gas extraction.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 15 - 45 µm15 - 45 µm
 15 - 53 µm15 - 53 µm
 53 - 120 µm53 - 120 µm
 53 - 150 µm53 - 150 µm
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.5 - 7.1 %5.5 - 7.1 %
Carbon, C <= 0.080 %<= 0.080 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.25 %<= 0.25 %
Molybdenum, Mo 0.50 - 2.0 %0.50 - 2.0 %
Nitrogen, N <= 0.050 %<= 0.050 %
Other, each 0.10 %0.10 %
Other, total 0.30 %0.30 %
Oxygen, O <= 0.15 %<= 0.15 %
Titanium, Ti 84.905 - 91.4 %84.905 - 91.4 %
Vanadium, V 0.80 - 2.5 %0.80 - 2.5 %
Zirconium, Zr <= 0.15 %<= 0.15 %
 1.5 - 2.5 %1.5 - 2.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMXCK1096 / 299727

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.