MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Saint-Gobain COHRlastic® 1115 Abrasion Resistant Silicone Coated Fabric
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thin and tough, dimensionally stable yet flexible. T Their many applications include belting, vacuum blankets, thermal shielding and diaphragms. The 1000 series has superior electrical properties and good abrasion resistance, while the 3000 series has a smoother, more compressible coating for gasketing applications. SGPPL also has extensive special order capabilities. All data based on a 0.007 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.335 g/cc1.335 g/ccWoven Density
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break <= 10 %<= 10 %ASTM D374
Flexural Strength 3.45 MPa500 psiBurst Strength
Tear Strength Test 2020lbm Strength in Fill/Transverse direction
 2222lbm, for strength in Warp/Longitudinal direction
Tear Strength 31.6 kN/m180 pliFill/Transverse direction
 35.1 kN/m200 pliWarp/Longitudinal direction; ASTM D1000
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
 
Descriptive Properties
ColorRed-Brown
Thread Count (Fill)32
Thread Count (Warp)42
Weight (oz/yd^2)15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber
A. Schulman BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound
CHT Group QSil 553 QSI Quantum Silicones Silicone Potting Material
CHT Group QSil 550SB QSI Quantum Silicones Self-Priming Silicone Potting Material
CHT Group QGel 300 QSI Quantum Silicones High Strength Gel

PSTGQZ283 / 68797

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.