MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Nouryon Berolamine 10 (BA-10) Triethanolamine
Categories: Other Engineering Material

Material Notes: Reaction mass of triethanolamine, diethanolamine and tri-hydroxyethylethylenediamine. BA-10 contains a high level of triethanolamine and is mainly used as a grinding agent for cement to reduce energy consumption.

CAS number: 102-71-6 (TEA)

EINECS/ELINCS No.: 203-049-8

Molecular formula: C6H15NO3

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³
pH 11115% solution
Viscosity 934 cP934 cPDynamic viscosity
Molecular Weight 149.1 g/mol149.1 g/mol
Vapor Pressure 9.00e-8 bar0.0000675 torr
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 23.0 °C
@Pressure 0.1013 MPa
<= 73.4 °F
@Pressure 14.69 psi
Boiling Point 336 °C
@Pressure 0.1013 MPa
637 °F
@Pressure 14.69 psi
Flash Point 179 °C
@Pressure 0.1013 MPa
354 °F
@Pressure 14.69 psi
Ignition Temperature >= 170 °C>= 338 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.50 %<= 0.50 %
 
Descriptive Properties
AppearanceLight brown liquid
ColorDark
Content= 0.5%Monoethanolamine (MOA 568)
 = 30%Diethanolamine (MOA 568)
 = 30%Higher ethanolamines (MOA 568)
 = 50%Triethanolamine (MOA 568)
OdorAmmonical
Partition coefficient-1N-octanol/water, 25°C, log Pow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY429 / 285952

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.