MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

EMS-Grivory Grilon® BM-30 FR Nylon 6, 30% Mineral Fiber Reinforced, Flame Retardant, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Mineral Filled

Material Notes: Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Filler/Reinforcement: Mineral, 30% Filler by Weight

Additive: Flame Retardant

Features: Flame Retardant; Flame Retardant; UV Resistant

Uses: Connectors; Electrical/Electronic Applications

RoSH Compliance: RoSH Compliant

Forms: Granules

Processing Method: Injection Molding

Information provided by EMS-Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183
Water Absorption 3.0 %3.0 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 8.0 %8.0 %ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 84.8 MPa12300 psiISO 527-2
Tensile Strength, Yield 84.8 MPa12300 psiISO 527-2
Elongation at Break 2.5 %2.5 %Nominal; ISO 527-2
Elongation at Yield 3.0 %3.0 %ISO 527-2
Tensile Modulus 6.40 GPa928 ksiISO 527-1
Charpy Impact Unnotched  3.57 J/cm²
@Temperature -30.0 °C
17.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 3.99 J/cm²
@Temperature 22.8 °C
19.0 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.199 J/cm²
@Temperature -30.0 °C
0.950 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.294 J/cm²
@Temperature 22.8 °C
1.40 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.2 µm/m-°C39.0 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 79.2 µm/m-°C44.0 µin/in-°FISO 11359-2
Melting Point 222 °C432 °F10ºC/min; ISO 11357-3
Maximum Service Temperature, Air 80.0 - 110 °C176 - 230 °FLong Term; ISO 2578
 160 °C320 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FUnannealed; ISO 75-2/A
Deflection Temperature at 8.0 MPa 50.0 °C122 °FUnannealed; ISO 75-2/C
Flammability, UL94 V-2
@Thickness 0.762 mm
V-2
@Thickness 0.0300 in
IEC 60695-11-10,-20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRIM420 / 307779

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.