MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eastman Provista ST Copolymer
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Provista Copolymer ST is a resin specifically developed for profile extrusion where high clarity and gloss, toughness, and processability are critical. Provista Copolymer ST is a second-generation material that complements Provista by offering similar features, while providing greater toughness. Provista Copolymer ST is ideal in applications that place greater physical demands on the profile.

Applications/Uses

  • Packaging tubes
  • Pricing channels
  • Signage channels
  • Plastic angle moldings
  • Profiles
  • Store fixtures
  • Key Attributes

  • Ease of processing
  • Excellent chemical resistance
  • Meets FDA regulations for food contact
  • Sparkling clarity and high gloss
  • Toughness with flexibility
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 1.25 g/cc1.25 g/ccASTM D792
    Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM D955
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Rockwell R 105105ASTM D785
    Tensile Strength at Break 48.0 MPa6960 psiASTM D638
    Tensile Strength, Yield 47.0 MPa6820 psiASTM D638
    Elongation at Break 300 %300 %ASTM D638
    Elongation at Yield 5.0 %5.0 %ASTM D638
    Tensile Modulus 1.90 GPa276 ksiASTM D638
    Flexural Strength 65.0 MPa9430 psiASTM D790
    Flexural Modulus 1.90 GPa276 ksiASTM D790
    Izod Impact, Notched  0.630 J/cm
    @Temperature -40.0 °C
    1.18 ft-lb/in
    @Temperature -40.0 °F
    ASTM D256
     NB
    @Temperature 23.0 °C
    NB
    @Temperature 73.4 °F
    ASTM D256
    Izod Impact, Unnotched NBNBASTM D4812
     NB
    @Temperature -40.0 °C
    NB
    @Temperature -40.0 °F
    ASTM D4812
    Puncture Energy 41.0 J30.2 ft-lbPuncture Resistance @Max Load, 0°C; ASTM D3763
     41.0 J30.2 ft-lbPuncture Resistance @Max Load, 23°C; ASTM D3763
     39.0 J
    @Temperature -40.0 °C
    28.8 ft-lb
    @Temperature -40.0 °F
    Puncture Resistance at Max Load; ASTM D3763
     
    Thermal PropertiesMetricEnglishComments
    Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C163 °FASTM D648
    Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C145 °FASTM D648
    Vicat Softening Point 85.0 °C185 °FASTM D1525
     
    Optical PropertiesMetricEnglishComments
    Haze 1.3 %1.3 %ASTM D1003
    Gloss 143 %143 %at 60°; ASTM D2457
    Transmission, Visible 87 %87 %Regular Transmittance; ASTM D1003
     91 %91 %Total Transmittance; ASTM D1003
     
    Descriptive Properties
    Color, CIE a*-0.2VGAS-A-AN-G-RS-001
    Color, CIE b*0.6VGAS-A-AN-G-RS-001
    Color, CIE L*95VGAS-A-AN-G-RS-001

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Eastman Eastar DN004 PCTG Copolyester
    Eastman Eastar™ 6763 Copolyester
    Eastman Eastar DN011 Copolyester
    Eastman Eastar DN010 Copolyester
    Eastman Eastar BR003 Natural PCTA Copolyester

    PE9094 / 35150

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.