MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lotte Advanced Materials Titanvene™ LL3840UA LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Titanvene™ LL3840UA is a butene co-polymer based linear low density polyethylene which has been specially developed for manufacturing large containers. Titanvene™ LL3840UA offers excellent UV resistance (UV6) for outdoor exposure with high levels of UV light radiation where the use of inorganic pigments or carbon black is normally recommended.

Applications: Titanvene™ LL3840UA is designed for large rotational molding containers, traffic cone and garbage bin.

Information provided by Lotte Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.936 g/cc0.0338 lb/in³ISO 1183 Method D
ESCR 10% Igepal® 300 hour300 hourF50; ASTM D1693
Melt Flow 4.00 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.00 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133 Condition 4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 62.062.0ISO 868 Type D
Tensile Strength, Yield 17.0 MPa2460 psiType 2 Speed C; ISO/R 527
Elongation at Break 1600 %1600 %Type 2 Speed C; ISO/R 527
Flexural Modulus 1.10 GPa159 ksiISO 178
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²ISO 179 Type 1 Notch A
 
Thermal PropertiesMetricEnglishComments
Melting Point 125 °C257 °FISO 3146 Method C
Vicat Softening Point 117 °C243 °FISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOTT9612 / 326094

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.