MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Go Yen Chemical GOYENCHM-AP750 Nanometer Special Innovation treated by silicone grade Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Advantages:
  • Belong to non-halogen flame retardant (no fluorine, chlorine, bromine or other halogen )
  • Cause less amount of Smoke while end-products ignited
  • Provide strong thermal decomposition
  • With excellent long-term flame-resistant ability
  • Won’t affect physical properties of resins and plastic.
  • With good compatibility with multi-kinds polymers, resins, plastic, elastomer ,adhesives.
  • Offer excellent flame retardant effect
Applications:
  • PE(HDPE,LDPE), PP, POLYOLIFIN, PET,NYLON,POM, Engineering Plastic….etc.
  • Coatings and Various Resins: Flame Retardant paints, all kinds of Acrylic related products, PU, PMMA, Latex, Adhesives
  • Phenol, Epoxy, Unsaturated Polyester, Polyester resin , melamine, Acrylic resin…etc.
  • Rubber industry : EPDM, CR, NBR, SBR, SIR, CSM, NR.IIR, various kinds of flame retardant rubber.
  • Elastomer: TPE, TPU, SBS, SEBS, TPR, TPV, various kinds of elastomer.
  • Foam Polymers: Applied in multi-kinds of foam Products, especially Rigid PU Foam Polymers, EVA foam materials.
  • Others: Printing Ink, paper, furniture plywood, Pigment, printing, backing glue, flame retardant master batch, textile, various kinds of flame retardant for electronic products.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solubility in Water <= 0.10 %<= 0.10 %10% suspension
Particle Size 15 µm15 µm
pH 6.5 - 8.56.5 - 8.5
Viscosity <= 10 cP<= 10 cP10% suspension
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 1.0<= 1.0mg KOH/g
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature >= 300 °C>= 572 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.25 %<= 0.25 %
 
Component Elements PropertiesMetricEnglishComments
Nitrogen, N 14 - 15 %14 - 15 %
Phosphorus, P 31 - 32 %31 - 32 %
 
Descriptive Properties
AppearanceFine powder
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN108 / 266416

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.