MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ortofon OM 1097 Rubber type: Chloroprene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Special properties:
  • Aging and heat resistance
  • Resistance to biological factors (fungi and soil bacteria)
  • Low gas permeability
  • Good electrical properties /ul>Applications:
    • Membranes
    • Dampers
    • Hearing aids
    • Bellows and dust caps
    • General purpose seals

    Information provided by Ortofon A/S

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 - 1.54 g/cc0.0542 - 0.0556 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 47 - 5747 - 57ISO 7619-1
Tensile Strength 11.0 MPa1600 psiISO 37
Elongation at Break 600 %600 %ISO 37
Compression Set 27 %
@Temperature 70.0 °C,
Time 86400 sec
27 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815
 
Descriptive Properties
ColorGrey
Range of temperature in dry air-10-100°C
Resistance to chemicals (acids/bases)Average
Resistance to hydrolysis (water and steam)Average
Resistance to mineral oil and gasAverage
Resistance to weather and ozoneGood
Wear resistanceGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PORTOM010 / 296213

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.